Artistic colored Granite Paint(Smooth Surface) process flow

Maydos granite texture stone paint

Granite Paint

1. Base surface treatment

2. Scrape and level putty

3. Scrape fine particles

4. Roll water-in-water primer

5. Groove division treatment

6. Spray colored intermediate paint

7. Spray water-in-water main material

8. Spray dustproof topcoat

Precautions

1. Please choose a professional Granite Paint construction team. An experienced construction team plays a key role in the quality of the project.

2. The quality of the base treatment and putty layer has a significant impact on the final decorative effect and performance. The construction of the next process must be qualified after the previous process.

3. The construction environment temperature below 5℃ will affect the composition structure of the water-soluble paint before solidification, so it is not suitable for construction under this temperature condition. When it is below 5℃, the product is strictly prohibited to be stored in the open air and should be kept indoors above 5℃. Construction should be avoided when the humidity is above 80%.

4. When the wall pH is greater than 10, use 5% hydrochloric acid water or oxalic acid water to clean it, and then use clean water to clean it until the wall pH is less than 10 before construction.

5. The uniform construction of colored mid-coat paint and the bottom cover are the prerequisites for ensuring the overall beautiful effect.

6. Water-based water paint cannot be stirred with a mixer before construction, and cannot be diluted with water. If precipitation is found, it can be poured 2 to 3 times.

7. A special spray gun should be used for construction. Before construction, a test coating should be carried out on the test board, and the formal construction can be carried out after the color and shape are confirmed.

8. The coating amount of the main material directly affects the quality of the coating and the decorative effect. Excessive spraying will cause sagging and blurred patterns. Too little use will result in granular patterns and rough surfaces, and the coating performance index is low.